Prague Med. Rep. 2013, 114, 22-34

https://doi.org/10.14712/23362936.2014.35

Evaluation of the Three-year Experience with All-ceramic Crowns with Polycrystalline Ceramic Cores

Lenka Vavřičková1,*, T. Dostálová2, J. Charvát3, M. Bartoňová3

1Department of Dentistry, Faculty of Medicine in Hradec Králové, Charles University in Prague and University Hospital Hradec Králové, Hradec Králové, Czech Republic
2Department of Paediatric Stomatology, Second Faculty of Medicine, Charles University in Prague and University Hospital Motol, Prague, Czech Republic
3Department of Oral and Maxillofacial Surgery, First Faculty of Medicine, Charles University in Prague and General University Hospital in Prague, Prague, Czech Republic

References

1. Chong, K. H., Chai, J., Takahashi, Y., Wozniak, W. (2002) Flexural strength of In-Ceram alumina and In-Ceram zirconia core materials. Int. J. Prosthodont. 15, 183–188.
2. Coelho, P. G., Silva, N. R., Bonfante, E. A., Guess, P. C., Rekow, E. D., Thompson, V. P. (2009) Fatigue testing of two porcelain-zirconia all-ceramic crown systems. Dent. Mater. 25, 1122–1127. <https://doi.org/10.1016/j.dental.2009.03.009>
3. Denry, I., Kelly, J. R. (2008) State of the art of zirconia for dental applications. Dent. Mater. 24, 299–307. <https://doi.org/10.1016/j.dental.2007.05.007>
4. Deville, S., Chevalier, J., Gremillard, L. (2006) Influence of surface finish and residual stresses on the ageing sensitivity of biomedical grade zirconia. Biomaterials 27, 2186–2192. <https://doi.org/10.1016/j.biomaterials.2005.11.021>
5. Fradeani, M., D’Amelio, M., Redemagni, M., Corrado, M. (2005) Five-year follow-up with the Procera all-ceramic crowns. Quintessence Int. 36, 105–113.
6. Goodacre, C. J., Campagni, W. V., Aquilino, S. A. (2001) Tooth preparations for complete crowns: an art form based on scientific principles. J. Prosthet. Dent. 85, 363–376. <https://doi.org/10.1067/mpr.2001.114685>
7. Heuer, A. H., Lange, F. F., Swain, M. V., Evans, A. G. (1986) Transformation toughening: an overview. J. Am. Ceram. Soc. 69, i–iv. <https://doi.org/10.1111/j.1151-2916.1986.tb07400.x>
8. Kaplan, E. L., Meier, P. (1958) Non parametric estimation from incomplete observation. J. Am. Stat. Assoc. 53, 457–465. <https://doi.org/10.1080/01621459.1958.10501452>
9. Kim, J. W., Covel, N. S., Guess, P. C., Rekow, E. D., Zhang, Y. (2010) Concerns of hydrothermal degradation in CAD/CAM zirconia. J. Dent. Res. 89, 91–95. <https://doi.org/10.1177/0022034509354193> <PubMed>
10. Malament, K. A., Socransky, S. S. (1999) Survival of Dicor glass-ceramic restoration over 14 years. Part II: Effect of thickness of Dicor material and design of tooth preparation. J. Prosthet. Dent. 81, 662–667. <https://doi.org/10.1016/S0022-3913(99)70104-6>
11. Piconi, C., Maccauro, G. (1999) Zirconia as a ceramic biomaterial. Biomaterials 20, 1–25. <https://doi.org/10.1016/S0142-9612(98)00010-6>
12. Pjetursson, B. E., Sailer, I., Zwahlen, M., Hämmerle, C. H. (2007) A systematic review of the survival and complication rates of all-ceramic and metal-ceramic reconstruction after observation period at least 3 years. Part I: Single crowns. Clin. Oral Implants Res. 18, 73–85 (Suppl. 3). <https://doi.org/10.1111/j.1600-0501.2007.01467.x>
13. Raigrodski, A. J. (2006) Materials for all ceramic restorations. J. Esthet. Restor. Dent. 18, 117–118. <https://doi.org/10.1111/j.1708-8240.2006.00003.x>
14. Ryge, G., Cvar, J. F. (1971) Criteria for clinical evaluation of dental restorative materials. US Dental Health Center, Publication No. 7902244, US Government Printing Office, San Francisco.
15. Sailer, I., Pjetursson, B. E., Zwahlen, M., Hämmerle, C. H. (2007) A systematic review of the survival and complication rates of all-ceramic and metal-ceramic reconstruction after observation period at least 3 years. Part II: Fixed dental prostheses. Clin. Oral Implants Res. 18, 86–96 (Suppl. 3). <https://doi.org/10.1111/j.1600-0501.2007.01468.x>
16. Sato, T., Shimada, M. (1984) Crystalline phase-change in yttria-partially-stabilized zirconia by low-temperature annealing. J. Am. Ceram. Soc. 67, C212–C213. <https://doi.org/10.1111/j.1151-2916.1984.tb09624.x>
17. Sato, T., Ohtaki, S., Shimada, M. (1985) Transformation of yttria partially stabilized zirconia by low temperature annealing in air. J. Mater. Sci. 20, 1466–1470. <https://doi.org/10.1007/BF01026344>
18. Subbarao, E. C. (1981) Zirconia – an overview. In: Science and Technology of Zirconia. Heuer, A. H., Hobbs, L. W., pp. 1–24, The American Ceramic Society, Columbus.
19. Tinschert, J., Schulze, K. A., Natt, G., Latzke, P., Heussen, N., Spiekermann, H. (2008) Clinical behavior of zirkonia-based fixed partial dentures made of DC-Zirkon: 3 years result. Int. J. Prosthodont. 21, 217–222.
20. Tyszblat Sadoun, M. (2001) inventor, A new all ceramic system, 1988. The Patents and Designs Journal 5872, EP0718592. EP95119818.3.